SPRING BACK CALCULATOR

Bend a test piece, measure it, and this calculator tells you the angle to program so your next part comes out on target. It works for stainless steel and any other sheet metal, because it uses your own measurements rather than textbook values.

Results are based on your test bend and assume the same material, thickness, tooling and bend radius for the production part. Always check the first production part.

How to use the spring back calculator

1. Make a test bend. Use an offcut of the same material, thickness and temper as your production part, with the same punch and die.
2. Enter the angle you programmed. This is the bend angle the press brake was set to, for example 90°.
3. Measure and enter the angle you got. Measure the part after it’s released from the tooling, with a protractor or angle gauge. For example, 85°.
4. Enter your target angle. This is usually the same as the angle you tested, but it can be different. If you tested at 90° and need a 120° bend, enter 120°.
5. Read your result. The calculator shows the spring back, the spring back factor (Ks), and the angle to program for your target.


Which angle to measure: The calculator uses the bend angle, meaning how far the sheet has been bent from flat. A right-angle bend is 90°. If your drawings use the included angle (the angle inside the bend, where a flat sheet is 180°), subtract it from 180° first. For example, a 135° included angle is a 45° bend angle.

Spring back calculator

Enter your test bend to find the angle to program.

°
°
°
Spring back–
Spring back factor (Ks)–
Angle to program–

Angles are bend angles measured from flat (a right-angle bend is 90°). Assumes the same material, thickness, tooling and radius as your test bend. Always check the first production part.

Understanding your result

The calculator gives you three numbers.
  1. Spring back is how far the bend opened after release: the angle you programmed minus the angle you measured. Program 90°, measure 85°, and spring back is 5°.
  2. Spring back factor (Ks) is the measured angle divided by the programmed angle. In the example, 85 ÷ 90 = 0.944. A Ks of 1 means no spring back; the lower it is, the more the bend opens. Ks is useful because it stays roughly constant for a given material, thickness and bend radius, even when the angle changes. Record it for each material and tool set-up you use.
  3. Angle to program is your target angle divided by Ks. For a 90° target, that’s 90 ÷ 0.944 = 95.3°. For a 120° target with the same set-up, it’s 127.1°.

Why not just add the spring back? Adding 5° to every bend works when your target is the same as your test angle. For a different target, spring back grows with the bend angle, so adding a fixed 5° would leave a 120° bend about 2° short. Dividing by Ks scales the correction to the angle.

Check the first part. Ks is a good guide, but tooling wear, batch-to-batch material variation and large changes in angle can all shift it. Measure the first production part and fine-tune if needed.

Typical spring back for stainless steel

No test piece yet? These typical figures give a starting point for your first bend. They vary with temper, batch and tooling, so always confirm with a test bend.
ConditionStainless Steel Spring Back (Approx. Angle)Notes
Minimum (tight bend)2o - 4oFor a tight bend where the inside radius is equal to the material thickness (Ri = 1t).
Moderate4o - 15oFor medium radii, such as Ri = 6t to Ri =20t for annealed 304 or 302 Stainless Steel.
Profound/large radiusExceeding to 30o - 60oOccurs in air forming when the inside radius is very large relative to the material thickness, often Ri is eight times or more than t.

At a tight bend (Ri = 1t), 304 stainless steel typically springs back 2–3°, compared with 0.75–1° for cold-rolled steel. Temper makes a large difference: half-hard 301 stainless can spring back several times more than annealed 304 at the same radius.
For mechanical properties by grade and temper, see our stainless steel data sheets.

How to reduce spring back

Overbending corrects spring back; these steps reduce it in the first place.

  • Choose a softer temper. Annealed stainless springs back far less than half-hard or work-hardened material.
  • Use a tighter bend radius. A lower inside radius relative to thickness puts more of the bend into permanent deformation.
  • Bottom or coin the bend. Pressing the sheet fully into the die gives less spring back than air bending.
  • Narrow the die opening. In air bending, a narrower opening gives a smaller radius and less spring back.
  • Use active angle control. CNC press brakes with angle measurement correct each bend automatically.
For the full explanation of why spring back happens and every way to manage it, read our guide: Avoiding Spring Back – How to Ensure Accurate Bends in Stainless Steel.

Less spring back starts with the right material

Overbending corrects spring back; these steps reduce it in the first place.

  • Choose a softer temper. Annealed stainless springs back far less than half-hard or work-hardened material.
  • Use a tighter bend radius. A lower inside radius relative to thickness puts more of the bend into permanent deformation.
  • Bottom or coin the bend. Pressing the sheet fully into the die gives less spring back than air bending.
  • Narrow the die opening. In air bending, a narrower opening gives a smaller radius and less spring back.
  • Use active angle control. CNC press brakes with angle measurement correct each bend automatically.
For the full explanation of why spring back happens and every way to manage it, read our guide: Avoiding Spring Back – How to Ensure Accurate Bends in Stainless Steel.

Want less spring back to correct?

Temper and grade are decided when you order material, long before the part reaches the press brake. Datum supplies precision 301 and 304 stainless steel strip and can manage bending, folding and crimping of your parts.

Prove it before production. We can make prototype parts in your chosen grade, so you can measure spring back before committing to tooling.

FAQ'S

Subtract the angle you measured after bending from the angle you programmed. If you program 90° and measure 85°, spring back is 5°.

By the amount it springs back on a test bend. For 304 stainless at a tight radius, that’s typically 2-3°, but larger radii and harder tempers need much more. Divide your target angle by the spring back factor to get the angle to program.

The ratio of the bend angle after release to the bend angle under load. A Ks of 0.95 means the bend relaxes to 95% of the angle you programmed.
Yes. Because it uses your own test bend, it works for aluminium, mild steel, copper, brass and other sheet metals.
Temper, batch-to-batch yield strength, thickness tolerance, die opening and tooling wear all affect spring back. That’s why a test bend on your own equipment is more reliable than published figures.